The Linkam Optical DSC450 is a DSC and microscope for thermal and glass transition measurements. It combines Differential Scanning Calorimetry (DSC) with light microscopy, which provides a wealth of information for characterizing polymers, pharmaceuticals and other materials.

The DSC stage mounts on a microscope, enabling high-resolution image and time recording of sample transitions. The system includes a T96 controller, LINK software and optional Digital Imaging and Thermal Analysis by Structural Characterization (TASC) modules.

Key Advantages at a Glance

  • Highly sensitive and accurate, with thermal transitions measured at low heating rates or with small sample sizes without loss of sensitivity and accuracy
  • Wide temperature range from -150 °C to 450 °C; the optional LNP96-S is needed for low temperatures
  • Simultaneous imaging and DSC analysis with the Linkam Imaging Station, optimized for the Linkam stage; the measurement chamber lid has a silica window for capturing and recording images
  • Optional TASC module (developed with Cyversa) that tracks changes in surface structure and shows glass and melting transitions with high accuracy
  • Analysis of different areas of the same sample to identify inhomogeneity
  • Modular thermal analysis system: TASC can be combined with any Linkam thermal stage
  • Sealed crucible available for closed-pan (cup-lid) experiments

Suitable For

The DSC450 is suited to measuring and imaging glass transitions and melting peaks for many applications, including:

  • Measurement and imaging of glass transitions and melting peaks
  • Materials
  • Pharmaceutical products
  • Food

Ask Analis' local Benelux experts for more information, a demonstration, or a personalized quote.

    This combination does not exist.

    Données Techniques

    Category

    Specification

    Temperature range

    -150 °C to 450 °C

    Heating / cooling

    0.01 °C to 30 °C/min

    Stability

    <0.1 °C

    Lens working distance

    9.7 mm

    Sample pans

    Aluminium and sapphire

    Furnace lid

    Sapphire or silver

    TASC

    The TASC Image Analysis module is an optional module that offers new thermal analysis systems. Linkam and Cyversa have entered into a collaboration and developed a thermal technique for analyzing materials.

    • Turn your temperature-controlled microscope stage into a thermal analysis laboratory suitable for measuring glass and melting transitions in many different materials, including opaque samples.
    • More sensitive than standard DSC at low heating rates and for small samples.
    • Kinetic parameters over a wider range of heating rates than conventional methods.
    • Thermal analysis on specified areas (local).

    Related Stages and Accessories

    • LNP96 nitrogen cooler available for temperatures down to -180 °C
    • Microscope hot stages available for temperatures between -196 °C and 1500 °C
    • Linkam TST350 Tensile Stage enables tensile tests up to 200 N at temperatures from 196 °C to 350 °C under a controlled gas atmosphere; microscope images are recorded during the measurement
    • Humidity generator controls relative humidity between 10 and 90% up to 85 °C